Products
Water collector
Typical value: ≤0.01% (achieved through an asymmetric or honeycomb-type manifold)
Category:
Water Collector
Keywords:
Water Collector
Water collector Details
Core Performance Parameters
Bleach loss rate
Typical value: ≤0.01% (achieved using an asymmetric or honeycomb-type demister)
Design Optimization: Employing the BO-160/45 asymmetric mist eliminator or a honeycomb‑type mist eliminator to reduce the risk of droplet carryover.
Structural Type
Asymmetric demister: Suitable for counterflow cooling towers, it enhances airflow turbulence and improves water collection efficiency.
Honeycomb mist eliminator: Integrated into the crossflow cooling tower packing to reduce droplet‑induced noise.
Applicable System Parameters
Operating pressure
Inlet pressure: 6.2×10⁴ Pa (approximately 62 kPa, matching the tower’s pressure rating)
Spray pressure: Low-pressure water distribution system (0.03–0.15 MPa), reducing the load on the mist eliminator.
Material Properties
Demister material: ABS or fiberglass (balancing corrosion resistance and structural strength)
Sealed Design: Leak-proof interface, suitable for acidic water applications (pH ≥ 1.0).
Demister and tower matching parameters
Model Example
DFNL Series:
Demister type: shallow‑pool type (DP type), deep‑pool type (GP type)
Structural height: 4,890 mm for the shallow‑tank type and 5,190 mm for the deep‑tank type (DFNDP/DFNGP‑100 model).
RT-300L/SB model:
The tower height is 3,600 mm, and the mist eliminator is integrated into the upper section of the tower.
Operational Metrics
Drift water humidity: After water collection, the relative humidity of the air drops below saturation.
Maintenance Schedule: Regularly remove blockages (e.g., water‑borne impurities ≤ 10 mm) to maintain efficiency.
Key Selection Points
Parameter |
Reference Values/Design Recommendations |
Applicable Scenarios |
Bleaching loss rate |
≤0.01% |
Areas with stringent environmental requirements (such as residential areas) |
Demister type |
Asymmetric type (counterflow tower) / Honeycomb type (crossflow tower) |
Select according to the cooling tower structure. |
Corrosion resistance |
ABS or fiberglass material |
Acidic water (pH ≥ 1.0) environment |